Polymer Property : Thickness = 254 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 25.4 - 254 microns
1.00 - 10.0 mil
Average value: 127 microns Grade Count:7
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Thickness 76.2 - 254 microns
3.00 - 10.0 mil
Technetics Group PLASTOLON™ Low Density PTFE Tape  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Thickness 203 - 254 microns
8.00 - 10.0 mil
Overall
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
Thickness 178 - 254 microns
7.00 - 10.0 mil
Overall
Arlon 910-10RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Thickness 203 - 254 microns
8.00 - 10.0 mil
Overall
Arlon 44560R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
Thickness 25.4 - 254 microns
1.00 - 10.0 mil
Technetics Group PLASTOLON™ Skived PTFE Tape  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)