Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 216 microns | 8.50 mil | |
Hexcel® HexForce™ 1581 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 216 microns | 8.50 mil | |
Hexcel® HexForce™ 7635 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 216 microns | 8.50 mil | ASTM D645 |
3M 6147 Performance Reinforced Water Activated Tape 3M™ Performance Reinforced Water Activated Tape 6147 is used for box sealing and other packaging applications. This has a fiberglass reinforced paper backing and a high tack water activated adhesiv.. |
|||
Thickness | 216 microns | 8.50 mil | Side 2 Layer 2; Arlon SQA-TMS-003 |
Arlon 55578GA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Thickness | 216 microns | 8.50 mil | Side 2 Layer 2; Arlon SQA-TMS-003 |
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Thickness | 216 microns | 8.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa.. |
|||
Thickness | 216 microns | 8.50 mil | Overall thickness |
Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should .. |
|||
Thickness | 216 microns | 8.50 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44576R009A 0.0058" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma.. |
|||
Thickness | 216 - 267 microns | 8.50 - 10.5 mil | Overall |
Arlon 47576R009 0.0095" (0.241 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data sho.. |
|||
Thickness | 216 microns | 8.50 mil | Overall Thickness |
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not.. |
|||
Thickness | 216 microns | 8.50 mil | |
3M Scotch® Super 88 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape Super 88 is a premium grade, 8.5 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is.. |
|||
Thickness | 216 - 241 microns | 8.50 - 9.50 mil | Adhesive and protective top covering |
3M 3635-100 Light Enhancement Film A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other.. |
|||
Thickness | 216 microns | 8.50 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |