Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Side 1
12.7 microns
0.500 mil
Side 2
191 microns
7.50 mil
Substrate
216 microns
8.50 mil
Overall thickness
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Silicone Property
Tensile Strength >= 5.52 MPa
>= 800 psi
Silicone Property
Elongation at Break >= 250 %
>= 250 %
Silicone Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test 3.0
3.0
Char Length, inches; FTMS 191A; Method 5903
25
25
Flame and Glow Time, seconds; FTMS 191A; Method 5903
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Aluminum
Total Product Weight (oz/yd2) 7.4
Uncoated Fabric Break Strength (lb/in) 200
Fill Direction
250
Warp Direction