Polymer Property : Thickness = 18.5 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 394 - 470 microns
15.5 - 18.5 mil
Overall
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..