Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 394 - 470 microns | 15.5 - 18.5 mil | Overall |
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |