Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 430 microns | 16.9 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 429 microns | 16.9 mil | |
Hexcel® HexForce™ GA130 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 430 microns | 16.9 mil | |
Zoltek Pyron® Plain Weave Fabric Oxidized Pan Fiber Oxidized Pan FiberApplications include: Industrial Flame and Thermal Insulation |