Zoltek Pyron® Plain Weave Fabric Oxidized Pan Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Pyron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Pyron® Plain Weave Fabric Oxidized Pan Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxidized Pan FiberApplications include: Industrial Flame and Thermal Insulation
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
Filament Diameter 12.5 µm
12.5 µm
Thickness 430 microns
16.9 mil
730 microns
28.7 mil
Component Elements Properties Metric English Comments
Carbon, C 62 %
62 %
Descriptive Properties Value Comments
Areal Weights, g/m2 190
359
Construction Plain Weave
Roll Length, m 150
45
Width, mm 1350
990
Yarn Input 2/10
2/27