Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 1 |
Arlon R35061R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 2 |
Arlon R35061R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | with adhesive |
3M Scotchcal™ 8171 Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | with adhesive |
3M Scotchcal™ 8174 Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | with adhesive |
3M Scotchcal™ 8674 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | with adhesive |
3M Scotchcal™ IJ8171 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Thickness | 81.3 - 152 microns | 3.20 - 6.00 mil | Dry |
3M Scotchkote™ EA5WB WB Epoxy Coating 3M Scotchkote WB Epoxy Coating EA5WB is a member of the expanding range of 3M Scotchkote high performance coating. It has been specifically developed for original equipment manufacture, particularly.. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 1 |
Arlon 51571R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum on fiberglass clothThis data Represents typical values for the production material. .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 2 |
Arlon 51571R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum on fiberglass clothThis data Represents typical values for the production material. .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 1 |
Arlon 51571S020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 2 |
Arlon 51571S020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 1 |
Arlon 51971R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 2 |
Arlon 51971R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 102 - 152 microns | 4.00 - 6.00 mil | Side 1 |
Arlon R31861R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 102 - 152 microns | 4.00 - 6.00 mil | Side 2 |
Arlon R31861R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 102 - 152 microns | 4.00 - 6.00 mil | Overall |
Arlon R34260N005 0.005" (0.127 mm) Unsupported/Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured Rubber Appearance: Clear gum on release linersThis data Represents typical values for the production material. The data should not be used to write, o.. |
|||
Thickness | 102 - 152 microns | 4.00 - 6.00 mil | Side 1 |
Arlon R34260N005 0.005" (0.127 mm) Unsupported/Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured Rubber Appearance: Clear gum on release linersThis data Represents typical values for the production material. The data should not be used to write, o.. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | with adhesive |
3M Scotchcal™ 8671 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |