Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3600 microns | 142 mil | Sheet; Internal |
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Thickness | 3600 microns | 142 mil | Sheet; Internal |
Azdel Plus C401-B01 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Thickness | 3600 microns | 142 mil | Sheet; Internal |
Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |