Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 183 - 335 microns | 7.20 - 13.2 mil | Wet |
3M Scotchkote™ EA5WB WB Epoxy Coating 3M Scotchkote WB Epoxy Coating EA5WB is a member of the expanding range of 3M Scotchkote high performance coating. It has been specifically developed for original equipment manufacture, particularly.. |