Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 183 microns | 7.20 mil | |
Hexcel® HexForce™ 160 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 183 microns | 7.20 mil | Typical; ASTM D374 |
DuPont™ Nomex® 410 Paper, 7 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 183 microns | 7.20 mil | Total; ASTM D3652 |
3M 438 Premium Performance Aluminum Foil Tape Thickest non-reinforced aluminum tape for heat resistance; smooth easy unwind; clean, straight edges with minimal wrinkling. UL 723 Classified.Information provided by 3M |
|||
Thickness | 183 - 335 microns | 7.20 - 13.2 mil | Wet |
3M Scotchkote™ EA5WB WB Epoxy Coating 3M Scotchkote WB Epoxy Coating EA5WB is a member of the expanding range of 3M Scotchkote high performance coating. It has been specifically developed for original equipment manufacture, particularly.. |
|||
Thickness | 183 microns | 7.20 mil | Total; ASTM D3652 |
3M 477 Vinyl Tape 3M™ Vinyl Tape 477 is comprised of a conformable, transparent vinyl backing with a versatile rubber adhesive. It is an excellent tape to use where abrasion resistance, transparency, conformability .. |
|||
Thickness | 183 microns | 7.20 mil | |
Hexcel® HexForce™ 372 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |