Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 1090 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film
Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-07Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-07Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wr..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-07Bxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-10Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Thickness 889 - 1090 microns
35.0 - 43.0 mil
Overall
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported
Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In..
Copyright © lookpolymers.com All Rights Reserved