Thickness 940 microns
37.0 mil
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Thickness 940 microns
37.0 mil
Standard
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Thickness 940 microns
37.0 mil
Standard
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Thickness 940 microns
37.0 mil
Standard; Laminate
GrafTech GRAFOIL® TG-251 Standard Internal Combustion Laminate, Metal Reinforced
GRAFOIL® Grade TG-251 is GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, gasoline/diesel head..
Thickness 940 microns
37.0 mil
Total; ASTM D3752
3M 1532 Sandblast Stencil
3M™ Sandblast Stencil 1532 is a tan rubber sandblast stencil featuring a polyester liner for use in a variety of sandblasting protection applications, including pavers, stone and glass surfaces.Inf..
Thickness 940 microns
37.0 mil
Total; ASTM D3752
3M 1532S Sandblast Stencil
3M™ Sandblast Stencil 1532S is a tan rubber sandblast stencil featuring a polyester liner for use in a variety of sandblasting protection applications, including pavers, stone and glass surfaces.In..
Thickness 940 microns
37.0 mil
Total; ASTM D3752
3M 1532T Sandblast Stencil
3M™ Sandblast Stencil 1532T is a tan rubber sandblast stencil featuring a polyester liner for use in a variety of sandblasting protection applications, including pavers, stone and glass surfaces.In..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film
Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-07Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-07Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wr..
Thickness 940 microns
37.0 mil
Overall; Arlon SQA-TMS-003
Arlon R39118R037L 0.037" (0.940 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyester Release Liner Transfer Pressure Sensitive Adhesive: Silicone PSASide 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Cured Silicone Rubber..
Thickness 940 microns
37.0 mil
with liner
3M GM400 Gripping Material
3M™ Gripping Material GM400 is based on 3M’s proprietary micro-replicated technology. 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM..
Thickness 940 microns
37.0 mil
3M Nextel™ CF-40 Woven Fabric 550
Information provided by 3M
Thickness 940 microns
37.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-07Bxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap..
Thickness 940 - 1090 microns
37.0 - 43.0 mil
Overall
Arlon 940-10Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Thickness 940 microns
37.0 mil
3M Nextel™ AF-40 Industrial Woven Fabric 312