Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 46.2 microns | 1.82 mil | Wet Film |
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C) |