Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 0.800 - 1.20 microns | 0.0315 - 0.0472 mil | |
Eifeler Coatings Technology MoST™ Molybdenum disulfide PVD Coating MoST™-Molybdenum disulfide as solid lubricant is deposited frequently and successfully as a slide layer on hard coatings.Information provided by Eifeler Coatings Technology |