Eifeler Coatings Technology MoST™ Molybdenum disulfide PVD Coating

Category Ceramic , Sulfide/Chalcogenide , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name MoST™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology MoST™ Molybdenum disulfide PVD Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MoST™-Molybdenum disulfide as solid lubricant is deposited frequently and successfully as a slide layer on hard coatings.Information provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 0.800 - 1.20 microns
0.0315 - 0.0472 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 500 - 1000
500 - 1000
Coefficient of Friction 0.10
0.10
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 400 °C
752 °F
Descriptive Properties Value Comments
Color silver - gray