Physical Properties Metric English Comments
Thickness 0.100 - 0.150 microns
0.00394 - 0.00591 mil
Dow SiLK™ Y 120 Semiconductor Dielectric Resin
SiLK™ Y 120 has an average pore size of < 2nm and a range of 1-3 nm, porous SiLK™ resins enables continuous Tantulum PVD barriers for 65 nm technology and beyond. Information provided by Dow