Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3.17 - 25.4 microns | 0.125 - 1.00 mil | |
Chengdu Polyster KLX-G11 PC Film & Sheet PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant,.. |
|||
Thickness | 3.17 - 25.4 microns | 0.125 - 1.00 mil | |
Chengdu Polyster KLX-G42 PC Film & Sheet PC film, high transparency, one side is velvet the other side is matte.Information provided by Chengdu Polyster Co., Ltd. |