Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster KLX-G42 PC Film & Sheet

Category Polymer , Film , Thermoplastic , Polycarbonate (PC)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster KLX-G42 PC Film & Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC film, high transparency, one side is velvet the other side is matte.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption <= 0.40 %
<= 0.40 %
ASTM D570
Thickness 3.17 - 25.4 microns
0.125 - 1.00 mil
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 55.0 MPa
>= 7980 psi
ASTM D882
Elongation at Break >= 90 %
>= 90 %
ASTM D882
Modulus of Elasticity 2.00 GPa
290 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM D117
Vicat Softening Point 135 °C
275 °F
ASTM D1525
Brittleness Temperature -130 °C
-202 °F
ASTM D746
Flammability, UL94 V-2

@Thickness 0.500 mm
V-2

@Thickness 0.0197 in
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Shrinkage <= 0.30 %
<= 0.30 %
ASTM D1204
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 2.95

@Frequency 1.00e+6 Hz
2.95

@Frequency 1.00e+6 Hz
ASTM D150
2.98

@Frequency 60 Hz
2.98

@Frequency 60 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Arc Resistance >= 100 sec
>= 100 sec
ASTM D495
Copyright © lookpolymers.com All Rights Reserved