Cell Length 0.180 mm
0.00709 in
Zotefoams ZOTEK® F 40 HT LS PVDF Foam
Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..