Polymer Property : Melt Flow = 95.1 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 27.5 - 95.1 g/10 min
27.5 - 95.1 g/10 min
Average value: 50.8 g/10 min Grade Count:6
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..