Polymer Property : Melt Flow = 90.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.00 - 90.0 g/10 min
4.00 - 90.0 g/10 min
Average value: 31.9 g/10 min Grade Count:51
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Melt Flow 3.00 - 90.0 g/10 min
3.00 - 90.0 g/10 min
Average value: 18.9 g/10 min Grade Count:40
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..