Physical Properties Metric English Comments
Melt Flow 9.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
9.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 2313 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region...
Melt Flow 9.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
9.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi..
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Melt Flow 9.3 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.3 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Melt Flow 9.3 g/10 min

@Load 10.0 kg,
Temperature 250 °C
9.3 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2644 PPE+HIPS (Asia Pacific)
PPE/HIPS unfilled for auto application