Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 85 g/10 min @Load 2.16 kg, Temperature 190 °C |
85 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin IFs730-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Melt Flow | 85 g/10 min @Load 10.0 kg, Temperature 230 °C |
85 g/10 min @Load 22.0 lb, Temperature 446 °F |
|
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Flow | 85 g/10 min @Load 2.16 kg |
85 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 6.4. |
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has ex.. |