Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.0 - 84 g/10 min | 1.0 - 84 g/10 min | Average value: 26.2 g/10 min Grade Count:27 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |