Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.73 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.73 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |