Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 73.8 g/10 min @Load 5.00 kg, Temperature 275 °C |
73.8 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |