Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.579 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.579 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2520 XL2 POM Description: Is a POM, injection-molding grade with increased electrical conductivity, for applications with reduced mechanical requirements.Information provided by BASF |