Physical Properties Metric English Comments
Melt Flow 5.00 - 65.0 g/10 min
5.00 - 65.0 g/10 min
Average value: 16.8 g/10 min Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..