Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 64.2 g/10 min | 1.00 - 64.2 g/10 min | Average value: 15.1 g/10 min Grade Count:38 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |