Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 61.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
61.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Melt Flow | 61.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
61.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |