Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 11E573 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melt Flow | 6.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Melt Flow | 6.9 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.9 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AR9100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 6.9 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.9 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5111 PEI 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Melt Flow | 6.9 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.9 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Melt Flow | 6.9 g/10 min @Load 5.00 kg, Temperature 300 °C |
6.9 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX1712 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled high heat for auto interior |
|||
Melt Flow | 6.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 72D811 Sealing Resin DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion.. |
|||
Melt Flow | 6.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP25-0620 Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 6.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flam™ 0106 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 6.9 g/10 min @Load 5.00 kg, Temperature 300 °C |
6.9 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2934 PPE+PS (Asia Pacific) PPE+PS GF20% High Heat Non-FR |
|||
Melt Flow | 6.9 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.9 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AR9100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |