Multibase Multi-Flam™ 0106 PP Black Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Flam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flam™ 0106 PP Black Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
at Equilibrium; ASTM D570
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 6.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.7 MPa
4600 psi
ASTM D638
Elongation at Break 280 %
280 %
ASTM D638
Flexural Strength 42.1 MPa
6100 psi
ASTM D790
Flexural Modulus 1.63 GPa
236 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 0.326 J/cm
0.610 ft-lb/in
ASTM D256
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C
157 °F
Unannealed; ASTM D648
Vicat Softening Point 151 °C
303 °F
ASTM D1525
Flammability, UL94 V-0
V-0
0.125 in