Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.27 - 25.0 g/10 min | 6.27 - 25.0 g/10 min | Average value: 17.8 g/10 min Grade Count:13 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Melt Flow | 6.27 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |