Polymer Property : Melt Flow = 6.27 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 6.27 - 25.0 g/10 min
6.27 - 25.0 g/10 min
Average value: 17.8 g/10 min Grade Count:13
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Melt Flow 6.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
BASF Ultraform® N2720 M63 30% Mineral Filled POM
Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF