Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 58.4 g/10 min | 5.00 - 58.4 g/10 min | Average value: 16.9 g/10 min Grade Count:14 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |