Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.0 - 57 g/10 min | 3.0 - 57 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX A6310 BLK Thermoplastic Elastomer SEBS Product Information: BP Flex Thermoplastic Elastomers are based on SEBS polymers (Styrene-ethylene/butylene-styrene) providing increased oxidation and weather resistance, higher service temperatures.. |