Polymer Property : Melt Flow = 500 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 500 g/10 min
500 g/10 min
modified; ASTM D1238, ISO 1133
DuPont Elvax® 4310 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 4310 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.Applications:Elvax® 4310 resins can be used for the following applications: adhesives, ..
Melt Flow 500 g/10 min
500 g/10 min
Exxon Method
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications.
Melt Flow 500 g/10 min

@Load 5.00 kg,
Temperature 316 °C
500 g/10 min

@Load 11.0 lb,
Temperature 600 °F
ASTM D1283
Chevron Phillips Ryton® PR27 Polyphenylene Sulfide Resin  (discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
Melt Flow 500 g/10 min

@Load 2.16 kg,
Temperature 190 °C
500 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont Elvax® 410 Ethylene Vinyl Acetate
DuPont™ Elvax® 410 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 410 resins can be used for the following applications: adhesives, sealants..
Melt Flow 500 g/10 min

@Load 2.16 kg,
Temperature 190 °C
500 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® UL 7510 Adhesive Application Resin
Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s..
Melt Flow 500 g/10 min

@Load 2.16 kg,
Temperature 190 °C
500 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 7511 is a very high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt ad..