Physical Properties Metric English Comments
Melt Flow 6.00 - 43.5 g/10 min
6.00 - 43.5 g/10 min
Average value: 26.2 g/10 min Grade Count:3
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..