Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42.8 g/10 min @Load 10.0 kg, Temperature 240 °C |
42.8 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Conditioned) Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc.. |
|||
Melt Flow | 42.8 g/10 min @Load 10.0 kg, Temperature 240 °C |
42.8 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry) Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc.. |