Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 40.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
40.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 40.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
40.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1776A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 40.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
40.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1366C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 40.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
40.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2990 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 40.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
40.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2303 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (430000 ppm) Features: Good UV Resistance Uses: Sheet Forms: Pellets Processing Method: Blow M.. |
|||
Melt Flow | 40.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
40.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 40.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
40.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2585F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 40.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
40.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2590A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 40.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
40.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
Melt Flow | 40.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
40.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron AN450M Flame Retardant ABS Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali |
|||
Melt Flow | 40.0 g/10 min @Load 2.16 kg, Temperature 125 °C |
40.0 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2854T Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |