Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 40.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 40.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Monprene® MP-1709C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 40.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
40.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1776A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 40.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1366C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 40.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
40.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2990 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 40.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
40.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB2303 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (430000 ppm) Features: Good UV Resistance Uses: Sheet Forms: Pellets Processing Method: Blow M..
Melt Flow 40.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 40.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2585F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 40.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2590A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 40.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
40.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron AN450M Flame Retardant ABS
Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali
Melt Flow 40.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
40.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron AN450M Flame Retardant ABS
Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali
Melt Flow 40.0 g/10 min

@Load 2.16 kg,
Temperature 125 °C
40.0 g/10 min

@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
Teknor Apex Monprene® MP-2854T Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..