Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.05 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.05 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 3 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 4.05 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.05 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 3 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 4.05 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.05 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 3 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |