Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 36.0 g/10 min | 5.00 - 36.0 g/10 min | Average value: 12.7 g/10 min Grade Count:80 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Melt Flow | 1.00 - 36.0 g/10 min | 1.00 - 36.0 g/10 min | Average value: 12.2 g/10 min Grade Count:17 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |