Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 35.4 g/10 min @Load 2.16 kg, Temperature 250 °C |
35.4 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Melt Flow | 35.4 g/10 min @Load 2.16 kg, Temperature 250 °C |
35.4 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Melt Flow | 35.4 g/10 min @Load 2.16 kg, Temperature 250 °C |
35.4 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |