Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.10 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.10 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
S&E Specialty Polymers TufPrene™ EXC-11-016 405 Black SEBS Information provided by S&E Specialty Polymers |
|||
Melt Flow | 3.10 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |