Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufPrene™ EXC-11-016 405 Black SEBS

Category Polymer , Thermoplastic , Styrene-Butadiene , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer S&E Specialty Polymers
Trade Name TufPrene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufPrene™ EXC-11-016 405 Black SEBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.10 g/cc
1.04 - 1.10 g/cc
ASTM D792
Melt Flow 3.10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69.0 - 75.0

@Time 10.0 sec
69.0 - 75.0

@Time 0.00278 hour
ASTM D2240
Tensile Strength 18.3 MPa
2650 psi
ASTM D412
25.62 MPa

@Temperature 136 °C,
Time 605000 sec
3716 psi

@Temperature 277 °F,
Time 168 hour
Aged
Elongation at Break 732 %
732 %
ASTM D412
622.2 %

@Treatment Temp. 136 °C,
Time 605000 sec
622.2 %

@Treatment Temp. 277 °F,
Time 168 hour
Aged
100% Modulus 0.00308 GPa
0.446 ksi
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature <= -53.0 °C
<= -63.4 °F
ASTM D746
Oxygen Index 20.0 %
20.0 %
ASTM D2863