Physical Properties Metric English Comments
Melt Flow 2.86 - 29.6 g/10 min
2.86 - 29.6 g/10 min
Average value: 13.2 g/10 min Grade Count:20
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..