Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.86 - 29.6 g/10 min | 2.86 - 29.6 g/10 min | Average value: 13.2 g/10 min Grade Count:20 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Melt Flow | 2.86 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.86 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |