Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.2 - 26.4 g/10 min @Load 2.16 kg, Temperature 400 °C |
13.2 - 26.4 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1183 |
Gharda Chemicals GATONE™ 5400 PEEK, Medium Viscosity Grade
(discontinued **) Medium viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical prope.. |